Click to enlarge image |
General Specification
Shrink Ratio
Shrinkage Direction |
Immersion Condition(H2O) |
Unit |
Transverse Shrinkage |
100°C for 30sec |
45±5 |
Longitudinal Shrinkage |
100°C for 30sec |
7±3 |
Technical Data
Properties |
Properties |
Measured Value |
Unit |
Testing Method |
Tensile Strength |
510 |
kgf/cm2 |
ASTM D882 |
Elongation (Non-printed Tube) |
353 |
% |
ASTM D882 |
Tensile Strength After Aging |
3.3 |
kgf |
ASTM D1004 |
Glass Transition Temp. |
>80 |
°C |
|
Heat Varation Temp. |
75~80 |
°C |
|
Crystallization Temp. |
125~175 |
°C |
|
Melting Temp. |
240~245 |
°C |
|
Electrical |
Properties |
Measured Value |
Uniy |
Testing Method |
Insulation Resistance (DC 500V) |
8.7 x 105 |
ML |
KSC 2402 |
Volume Resistivity |
1.5 x 1016 |
Ohm.cm |
ASTM D257 |
Surface Resistivity |
2.0 x 1013 |
Ohm |
ASTM D257 |
Dielectric Breakdown Voltage |
6.8/80um |
KV |
KSC 2402 |
Dielectric Proof Voltage (AC 5000V x 1mm) |
No Problem |
|
KSC 2402 | * These values wre obtained by actual measurement of one sample. If Customer need more extra condition, Measured Value could be changed.
|
|
[ 연락처 정보 ] |
Company |
(주)하니상사 |
Address |
서울시 서초구 서초동 1695-5, 로펌애비뉴빌딩 501호 (우:137-883) 한국 |
Phone |
82 - 2 - 5925640 |
Fax |
82 - 2 - 5925641 |
Homepage |
www.hanicorp.co.kr |
Contact |
이현선 / 부장 |
|
|
|
|
|
|
|
|